汽车结构件低载强化后的疲劳断口特性 被引量:4

Fracture Characteristic of Automobile Structure Strengthening under Low Amplitude Load
在线阅读 下载PDF
导出
摘要 利用扫描电镜对某汽车前轴低载强化后的材料断口特性进行了研究,力图从微观上揭示低载强化的成因和机理。结果表明:适当的强化载荷使组织变得密实、均匀,断口的孔洞数量、直径以及二次裂纹明显减少,低载强化有效地延缓了疲劳裂纹萌生,降低了疲劳裂纹扩展速率,使疲劳强度和疲劳寿命都得到提高。 The fatigue strength and life of automobile structures can be obviously increased by strengthening under low amplitude load. The mechanism of strengthening under low amplitude load was studied through the observation of fracture cross section of auto parts by means of SEM. Under proper strengtheneing loading, the microstructure became dense and homogeneous. Moreover, the number and diameter of voids and the number of secondary cracks decreased obviously. The fatigue crack initiation and propagating rate were reduced by strengthening under low amplitude loading.
出处 《机械工程材料》 CAS CSCD 北大核心 2006年第6期17-19,73,共4页 Materials For Mechanical Engineering
基金 国家自然科学基金(50375101) 上海汽车工业科技发展基金(0329)
关键词 汽车结构件 断口特性 低载强化 automobile structure fracture cross-section characteristic low amplitude load strengthening
  • 相关文献

参考文献5

二级参考文献7

共引文献29

同被引文献31

引证文献4

二级引证文献12

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部