摘要
炭浸提金工艺通常对磨矿细度要求较高(-200目90%),在夏家店金矿设计生产中,根据矿石性质,大胆采用了粗磨矿下炭浸提金,经实践证明完全达到了设计指标,大大降低了投资及生产成本。
The finer milling grain - size in the technology of gold leaching in cyanide carbon - in - pulp is required. But in Xiajiadian Gold Mine design, the technology of the coarse ore with gold in charcoal- in pulp was adopted. Stable indexes, low investment & operation cost, and remarkable benefit are achieved in the practical application of the technology.
出处
《中国钼业》
2007年第2期11-13,共3页
China Molybdenum Industry
关键词
炭浸
磨矿细度
试验
生产指标
leaching in carbon - in - pulp
milling grain - size
trial
technology indexes