用锌焙砂中浸渣制备铁精矿 被引量:2

Preparation of Iron Concentrate from Residue of Neutral Leaching of Zinc Calcine
在线阅读 下载PDF
导出
摘要 为综合利用湿法炼锌渣中的铁,进行了用锌焙砂中浸渣制备铁精矿的试验研究。试验在传统湿法炼锌工艺的基础上,将高酸浸出过程改为高温高酸还原浸出过程,使铁以亚铁形式进入溶液.最后用双氧水和碱式碳酸锌沉铁。试验结果表明,采用新工艺可从锌焙砂中浸渣制得含铁大于51%的铁精矿,使最终渣量大大减少,并且对锌和铟的回收率没有影响。 To comprehensively utilize the iron in the slag of wet zinc smelting, test is made on the preparation of iron concentrate from the residue of neutral leaching of zinc calcine. Based on the conventional wet zinc smelting process, the high acid leaching is transformed into high temperature high acid reduction leaching process, making it possible for the iron to enter the solution in the form of ferrous iron, which is then precipitated by hydrogen peroxide and basic zinc carbonate. The test results indicate that the new process can obtain an iron concentrate grading over 51% from the leaching residue of zinc calcine, greatly reducing the final residue amount and meanwhile having no impact on the recovery of both zinc and indium.
出处 《金属矿山》 CAS 北大核心 2007年第12期131-134,共4页 Metal Mine
关键词 湿法炼锌 中浸渣 高温高酸还原浸出 沉铁 Wet zinc smelting, Neutral leaching residue, High temperature high acid reduction leaching process, Iron precipitation
  • 相关文献

参考文献7

二级参考文献35

共引文献90

同被引文献19

引证文献2

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部