梅山重选车间2~0.5mm粒级铁矿物依靠湿式磁选机选别,工艺上总体比较稳定。为了提高回收率,对影响磁选机选别的因素进行分析优化,以提升2~0.5 mm粒级选别精度。
Meishan gravity sepration workshop 2-0.5 mm system' s iron ore are separated by the wet magnetic separator. In order to increase the recovery and the 2-0.5 mm system' s iron ore's quantity, the passage analysis the major influence of the magnetic separator.