摘要 以自制三羟甲基己烷为原料 ,采用自制的负载磷钨酸催化剂催化合成一系列三羟甲基己烷脂肪酸酯。通过大量实验研究了影响催化剂活性和酯化率的因素 ,筛选出最佳催化剂并确定了适宜的酯化工艺条件。最佳催化剂制备条件 :载体与活性物质量比 1/ 6 ,浸渍时间 5h ,烘焙温度 32 0℃。适宜的酯化工艺条件 :反应时间 12 0min ,反应温度2 2 0℃ ,压力 0 0 2~ 0 0 4MPa,催化剂质量分数 1 8%,庚酸 /三羟甲基己烷摩尔比 3 7/ 1 0。在此条件下酯化率可达96 0 %以上 ,而且催化剂可重复使用。通过质量检测及光谱分析 ,对目标产物进行了确证。 A series of trimethylolhexane triheptyl esters were synthesized from trimethylolhexane with special kinds of supported phosphotungstic acid catalyst. The factors affecting catalyst activity and esterification conversion were discussed, and the optimum conditions for catalyst and trimethylolhexane triheptyl esters preparation were obtained. The optimum conditions for catalyst preparation were: m(support)/m(active component), 1/6; impregnation time,5 h; baking temperature, 320 ℃. The optimum conditions for esterification were: reaction time, 120 min; reaction temperature, 220 ℃;mass fraction of catalyst, 1.8%; mole ratio of haptanone and trimethylolhexane,3.7/1.0. The esterification conversion reached over 96.0% under the optimum conditions. Moreover, the catalyst was used repeatedly. The product was also verified by quality test and spectroscopic analysis.
作者 郑敏 王作山
出处 《石油化工》 CAS CSCD 北大核心 2002年第7期551-554,共4页 Petrochemical Technology
关键词 催化合成 三羟甲基已烷 负载磷钨酸 三羟甲基已烷脂肪酸酯 酯化率 trimethylolhexane supported phosphotungstic acid trimethylolhexane triheptyl ester esterification conversion
  • 相关文献

参考文献1

同被引文献275

引证文献19

二级引证文献174

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部