摘要
分别采用氢氧化物共沉淀、碳酸盐共沉淀、喷雾干燥的方法合成了层状α-Na Fe O2结构的富锂正极材料0.5Li2Mn O3·0.5Li(Ni1/3Co1/3Mn1/3)O2,通过X射线衍射分析(XRD)、扫描电子显微镜(SEM)和电化学性能测试对不同合成方法所得的样品进行了表征。实验结果表明:氢氧化物共沉淀合成的前驱体所制备的正极材料0.5Li2Mn O3·0.5Li(Ni1/3Co1/3Mn1/3)O2具有良好的电化学性能,0.05C倍率下首次放电容量可达247.1 m A·h/g,0.2C倍率条件下经过50次循环,容量保持率为98.7%。
Layered Li-rich cathode material 0.5Li2MnO3 · 0.5Li (Ni1/3CO1/3Mn1/3)O2 with α-NaFeO/structure has been prepared by hydroxide co-precipitation, carbonate co-precipitation and spray drying methods respectively. The samples obtained by three methods were characterized by X-ray diffraction, scanning electron microscope and electrochemical characteristics analyses. The results show that the cathode material 0.5Li2MnO3 · 0.5Li (Ni1/3CO1/3 Mn1/3 )O2 synthesized by the hydroxide co-precipitation method presents excellent electrochemical performance, with the initial discharge capacity of 247.1 mA · h/g at 0.05C and the capacity retention of 98.7% after 50 cycles at 0.2C.
出处
《矿冶工程》
CAS
CSCD
北大核心
2014年第6期123-127,共5页
Mining and Metallurgical Engineering
基金
湖南省科技重大专项计划(2011FJ1005)