摘要 The desire for high-energy-density batteries calls for the revival of the Li metal anode.However,its application is hindered by enormous challenges associated with Li deposition/desolvation behaviors,such as side reactions,volume change,and dendrite formation.To overcome these challenges,Li deposition must be controlled to remain below the separator.Further,to enable longer cycle life,Li deposition should be constrained below the solid electrolyte interphase(SEI).To achieve these goals,it is critical to have a deep theoretical understanding and corresponding strategies.This paper examines Li plating/stripping in terms of behaviors,mechanisms,and influencing factors,and it proposes general strategies to control Li deposition.Comprehensive design strategies for the electrode,electrolyte,and their interface are essential.Three dimensional(3D)anodes are recommended to store most of the Li deposited below the surface of the anode.Artificial interface engineering can reduce the risk of Li deposition outside of the 3D anode,while electrolyte engineering favors Li transport,regulates Li deposition,and suppresses dendrites,serving as the final barrier to uncontrolled Li deposition.This paper reviews systemic theories and solutions to control Li deposition below the interface,paving the way for a promising route to build safer lithium metal batteries.
出处 《eScience》 2022年第1期47-78,共32页 电化学与能源科学(英文)
基金 This work was supported by funding from Natural Science Foundation of Beijing(grant no.Z20J00042) Beijing Municipal Science&Technology(grant no.Z191100004719001) National Natural Science Foundation of China(grant no.U196420104,U1932220,U2032107).
  • 相关文献

参考文献5

二级参考文献15

共引文献85

同被引文献128

引证文献11

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部