期刊文献+

金属材料在高温碳气氛中的结焦与渗碳行为 被引量:36

COKING AND CARBURIZING BEHAVIORS OF METAL MATERIALS IN HIGH TEMPERATURE CARBON-CONTAINING ATMOSPHERE
在线阅读 下载PDF
导出
摘要 叙述了碳气氛温度、金属材料种类及表面状态、构成碳源的气体种类、比例及流速等因素对金属材料结焦行为的影响 ,介绍了催化结焦的引发机理及其应用 .然后以FeCrNi合金为例 ,分别介绍了内部渗碳和金属粉化这两种渗碳行为 ,并叙述了温度、碳气氛、合金材料晶体结构及成分构成的影响 .最后分析了结焦和渗碳的关系 ,并介绍了添加结焦抑制剂、调整金属材料结构及成分构成、表面涂层化 3种防护对策 . This paper reviews some factors affecting the coking behaviors of metal materials,which are the temperature of the carbon-containing atmosphere,the kinds and the surface state of metal materials,and the kinds and ratio and flowing velocity of the gases forming the carbon-containing atmosphere,and then introduces the initiating mechanism of catalytic coking and its applications.Taking the Fe Cr Ni alloy as an example,the paper also respectively introduces two kinds of carburizing behaviors,i.e.inner carburizing and metal dusting,and then reviews the effects of temperature,carbon-containing atmosphere,as well as crystal structure and element constitution of the alloy on the inner carburizing and metal dusting.Finally the relations between coking and carburizing are analyzed,and three kinds of protective methods including adding coking inhibitor,adjusting structure and element constitution of metal materials,and preparing coating are introduced.
出处 《中国腐蚀与防护学报》 CAS CSCD 2004年第3期188-192,共5页 Journal of Chinese Society For Corrosion and Protection
基金 辽宁省优秀青年人才基金 中国石化总公司科技开发项目资助
关键词 金属材料 结焦 渗碳 金属粉化 metallic materials,coking,carburizing,metal dusting
  • 相关文献

参考文献25

  • 1[1]Baker R T K,Yates D J C,Dumesic J A.Mechanism of carbonformation during steam cracking of hydrocarbon[A].The182nd Meeting ofthe American Chemical Society[C].New York,1981,1-5
  • 2[2]Grabke H J.Carburization(A high temperature corrosion phenomenon)[M].MTI Publications,1998,No.52,1-4
  • 3[4]Lahaye J, Badie P, Ducret J.Mechanism of carbon formation during steam cracking of hydrocarbons[J].Carbon, 1977,15: 87 - 93.
  • 4[5]Tomaszewicz P, Jackson P R S, Trimm D L, Young D J.Morphological studies of coking on heat- resistant alloy[J] .J.Mater.Sci.,1985, 20: 4035 - 4044
  • 5[6]Jackson P R S, Trimm D L, Young D J.The coking kinetics of heat resistant austenitic steel in hydrogen- propylene atmospheres[J].J.Mater.Sci., 1986, 21:3125 - 3134
  • 6[7]Mitchell D R G, Young D J.A kinetic and morphologic study of the coking of some heat- resistant steels[J].J.Mater.Sci., 1994, 29:4357 - 4370
  • 7[10]Boehm H P.Carbon from carbon monoxide disproportion on nickel and iron catalyst: morphological studies and possible growth mechanisms[ J].Carbon, 1973, 11: 583 - 590
  • 8[11]Alstrup I.A new model explaining carbon filament growth on nickel, iron and Ni - Cu alloy catalysts[J].J.Catalysis, 1988, 109: 247- 251
  • 9[15]Baker R T K.Catalytic growth of carbon filaments[J].Carbon,1989, 27(3) :315 - 323
  • 10[16]Snoeck J W, Froment G F, Fowlea M.Filamentous carbon formation and gasification: thermodynamics driving force, nucleation and steady - state growth[J].J.Catalysis, 1997,169: 240 - 249

同被引文献330

引证文献36

二级引证文献102

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部