Block copolymers with different backbone compositions have been prepared by the condensation of dimethylamino terminated poly(dimethylsiloxane) (PDMS) and hydroquinone terminated poly(phthalazinone ether nitrile...Block copolymers with different backbone compositions have been prepared by the condensation of dimethylamino terminated poly(dimethylsiloxane) (PDMS) and hydroquinone terminated poly(phthalazinone ether nitrile) (PPEN) in the presence of chlorobenzcne/N-methyl pyrrolidone (NMP) as solvents. The products were characterized by FTIR, ^1H NMR and gel permeation chromatography. Differential scanning calorimetry analysis indicated that the block copolymers showed separated microphase.展开更多
A series of novel poly(aryl ether nitrile)s containing phthalazinone moiety were synthesized by the nucleophilic displacement reaction of bisphenol-like monomers (I) with 2,6-difluorobenzonitrile. The inherent vis...A series of novel poly(aryl ether nitrile)s containing phthalazinone moiety were synthesized by the nucleophilic displacement reaction of bisphenol-like monomers (I) with 2,6-difluorobenzonitrile. The inherent viscosities ranged from 0.46 to 1.07 dL g^-1. The glass transition temperatures were in the range of 277-295℃, and the temperatures for 10% weight loss in nitrogen atmosphere were found between 495 and 527 ℃. The structures of these resultant polymers were confirmed by FT-IR and 1^H NMR. Moreover, the properties of poly(aryl ether nitrile)s including solubility and crystallinity were also studied.展开更多
Chloromethylated poly(phthalazinone ether sulfone ketone) (CMPPESK) was prepared from poly(phthalazinone ether sulfone ketone) (PPESK) using chloromethyl octyl ethers (CMOE) with lower toxicity as chlorometh...Chloromethylated poly(phthalazinone ether sulfone ketone) (CMPPESK) was prepared from poly(phthalazinone ether sulfone ketone) (PPESK) using chloromethyl octyl ethers (CMOE) with lower toxicity as chloromethylated regent. CMPPESK was soluble in N-methyl-2-pyrrolidone (NMP), N,N-dimethylacetamide (DMAc) and chloroform. Quaternized poly(phthalazinone ether sulfone ketone) (QAPPESK) was prepared from CMPPESK by quaternization. QAPPESK had excellent solvent resistance, which was only partly soluble in sulfuric acid (98%) and swollen in N,N-dimethylformamide (DMF). The vanadium redox flow battery (V-RFB) using QAPPESK anion-exchange membrane had better performance with 88.3% of overall energy efficiency.展开更多
Two novel heterocyclic diamine monomers: 1,2-dihydro-2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl] (2H)phthalazin-1-one and 1,2-dihydro-2-(4-aminophenyl)-4-[4-(4-aminophenoxy)-3,5-dimethylphenyl](2H)phthalazin-1-one ...Two novel heterocyclic diamine monomers: 1,2-dihydro-2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl] (2H)phthalazin-1-one and 1,2-dihydro-2-(4-aminophenyl)-4-[4-(4-aminophenoxy)-3,5-dimethylphenyl](2H)phthalazin-1-one were successfully synthesized from readily available heterocyclic bisphenol-like monomers in two steps in high yield. A series of novel poly(aryl ether amide)s containing the phthalazinone moiety were successfully prepared by the direct polymerization of the novel diamines and aromatic dicarboxylic acids using triphenyl phosphite and pyridine as condensing agents.展开更多
A novel series of poly(aryl ether sulfone ketone)s (PPESKs) containing phthalazinone and biphenyl moieties were prepared by two-step nucleophilic polycondensation reaction. The ^-Mw values of these copolymers were...A novel series of poly(aryl ether sulfone ketone)s (PPESKs) containing phthalazinone and biphenyl moieties were prepared by two-step nucleophilic polycondensation reaction. The ^-Mw values of these copolymers were between 38,330 and 67,900. The glass transition temperatures (Tg) and 5% decomposition temperatures were ranged in 253-269 ℃ and 488-500 ℃, respectively, The structures of these copolymers were confirmed by FT-IR and ^1H NMR. Moreover, all the resultant copolymers were amorphous determined by wide angle X-ray diffraction (WAXD).展开更多
1, 2-Diliydro-4-(4-hydroxyphenyl)(2H)phthalazin-1-one(DHPZ) was sulfonated in concentrated Sulfuric acid. Poly(phthalazinone ether ketone) containing pendant sodium sulfonate group was synthesized from sulfonated and ...1, 2-Diliydro-4-(4-hydroxyphenyl)(2H)phthalazin-1-one(DHPZ) was sulfonated in concentrated Sulfuric acid. Poly(phthalazinone ether ketone) containing pendant sodium sulfonate group was synthesized from sulfonated and pure 1,2-dihydro-4-(4-hydroxyphenyl)(2H)phthalazin-1-one, and 4,4'-difluorodiphenylketone. The sulfonated monomer and sulfonated polymer were characterized with FT-IR and H-1-NMR.展开更多
Three novel poly(ether imide)s were synthesized by one-step solution polymerization from 2-(3, 4-dicarboxyl-N-phenyl)-4-(3, 4-dicarboxyl-phenoxyl-4-(2-methyl)-phenyl)-2, 3- phthal-azin-1-one dianhydride and three amin...Three novel poly(ether imide)s were synthesized by one-step solution polymerization from 2-(3, 4-dicarboxyl-N-phenyl)-4-(3, 4-dicarboxyl-phenoxyl-4-(2-methyl)-phenyl)-2, 3- phthal-azin-1-one dianhydride and three amines, and characterized. The polymers show good solubility and thermal properties.展开更多
Trimethoxysilyl-functionalized PPEK(PKGS) films had been designed to serve as wear resistant coatings for silicon surfaces. These surface films were formed by a dip-coating technique applied to self-assembled monola...Trimethoxysilyl-functionalized PPEK(PKGS) films had been designed to serve as wear resistant coatings for silicon surfaces. These surface films were formed by a dip-coating technique applied to self-assembled monolayers(SAMs).The formation and wetting behavior of PKGS films were characterized by means of contact angle measurement.The friction coefficient of the film prepared is very low(about 0.1),and the anti-wear behavior is good,with a lack of failure after sliding over 1800 s.展开更多
A novel poly(ether imide)s containing phthalazinone and isopropyl moieties derived from 2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl]-phthalazin-1-one and bisphenol-A diphthalic anhydride was synthesized by one-step ...A novel poly(ether imide)s containing phthalazinone and isopropyl moieties derived from 2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl]-phthalazin-1-one and bisphenol-A diphthalic anhydride was synthesized by one-step solution condensation polymerization in nr-cresol. The polymer was characterized by FTIR, NMR, molecular weights, glass transition temperature, thermal degradation temperature and WAXD.展开更多
A novel alkoxysilyl-functionalized poly(phthalazinone ether ketone) (PPEK) was prepared for the boundary lubricant application in micro-electro-mechanical system (MEMS). The synthesis of functionalized PPEK was starte...A novel alkoxysilyl-functionalized poly(phthalazinone ether ketone) (PPEK) was prepared for the boundary lubricant application in micro-electro-mechanical system (MEMS). The synthesis of functionalized PPEK was started from the hydroxylation of PPEK, then following with the corresponding ring-opening reaction of 3-glycidoxypropyltrimethoxysilane (GPTMS). The structures of the functional PPEK were confirmed by FTIR, 1H NMR, 29Si NMR, and UV–vis spectrum.展开更多
Based on several unsymmetrical, twist, noncoplanar phthalazinone-containing monomers 2a-2e and an active bis(4-fluorophenyl)phenyl phosphine oxide (BFPPO) monomer, a series of novel poly(phthalazinone ether phosp...Based on several unsymmetrical, twist, noncoplanar phthalazinone-containing monomers 2a-2e and an active bis(4-fluorophenyl)phenyl phosphine oxide (BFPPO) monomer, a series of novel poly(phthalazinone ether phosphine oxide)s (PPEPO) was synthesized by anhydrous K2CO3 mediated N-C coupling reaction in DMAc. The polymers exhibited good thermal properties with Tgs ranging from 267℃ to 306℃ and 5% weight loss temperatures in nitrogen higher than 430℃, together with high char yield upon prolonged heating at 800℃ (35%-56%). Moreover, the polymers were readily soluble in common organic solvents, such as N-methyl-2-pyrrolidone, chloroform and m-cresol. These polymers had inherent viscosities in the range of 0.45-0.72 dL/g and could be cast into flexible and colorless films by spin coating or casting approach.展开更多
A novel aromatic diamine, 1, 2-dihydro-2-(4-aminophenyl)-4-[3-methoxy-4-(4-aminophenoxy)]-2, 3-phthalazin-l-one (OO-DA) containing aza heterocyclic structure was synthesized from the bisphenol-like monomer in tw...A novel aromatic diamine, 1, 2-dihydro-2-(4-aminophenyl)-4-[3-methoxy-4-(4-aminophenoxy)]-2, 3-phthalazin-l-one (OO-DA) containing aza heterocyclic structure was synthesized from the bisphenol-like monomer in two steps and used for preparing new aromatic polyamides with high inherent viscosity of 0.89-1.03 dL.g^-1. The structures of diamine and polymers obtained were confirmed by MS, PT-IR, WAXD and ^1H-NMR. The synthesized polymers exhibited high glass transition temperature in the range of 281-307℃ and good solubility in polar solvents.展开更多
Dielectric energy storage materials that are extensively employed in capacitors and other electronic devices have attracted increasing attentions amid the rapid progress of electronic technology.However,the commercial...Dielectric energy storage materials that are extensively employed in capacitors and other electronic devices have attracted increasing attentions amid the rapid progress of electronic technology.However,the commercialized polymeric and ceramic dielectric materials characterized by low energy storage density face numerous limitations in practical applications.In this study,we report the simultaneous enhancement of dielectric properties of poly(arylene ether nitrile)(PEN)through the incorporating of sulfonated PEN(SPEN)modified barium titanate nanorods(BTNR)(SPEN@BTNR)and hot-stretching.BTNR is synthesized using a two-step hydrothermal method,aminated with KH550,and then reacted with SPEN to form the cladding-modified SPEN@BTNR.Due to the intrinsic high permittivity of barium titanate(BT)and enhanced compatibility between SPEN@BTNR and PEN stemming from the cladding of SPEN,the dielectric constant and breakdown strength of SPEN@BTNR/PEN composite are as high as 14.0 at 103 Hz and 198.1 kV/mm at the doping amount of 15 wt.%,respectively.As a result,the energy storage density of SPEN@BTNR/PEN is increased to 2.43 J/cm^(3),compared with that of 0.82 J/cm^(3)for PEN.In addition,derived from the rearrangement of SPEN@BTNR and orientation of PEN after hot-stretching,the dielectric constant and breakdown strength of SPEN@BTNR/PEN with 15 wt.%fillers are further enhanced to 17.1 and 204.8 kV/mm,respectively,resulting in an energy storage density of 3.36 J/cm^(3).The boosting of energy storage density up to 310%provides a new idea for improving the performances of dielectric energy storage materials.展开更多
Sulfonated poly(ether ketone)s containing 3,5-dimethyl phthalazinone moieties (SPPEK-DMs) with different degrees of sulfonation (DS) were synthesized via direct polycondensation from 4-(3,5-dimethyl-4-hydroxyph...Sulfonated poly(ether ketone)s containing 3,5-dimethyl phthalazinone moieties (SPPEK-DMs) with different degrees of sulfonation (DS) were synthesized via direct polycondensation from 4-(3,5-dimethyl-4-hydroxyphenyl)-2,3- phthalazinone, 4,4'-difluorobenzophenone and 3,3'-disulfonate-4,4'-difluorobenzophenone. The chemical structure of SPPEK-DMs was characterized by FTIR and 1H-NMR. Thermal stability of SPPEK-DMs was characterized by the thermogravimetric analysis. The membranes prepared from SPPEK-DMs exhibited ion exchange capacities (IEC) ranging from 0.93 mmol.g-1 to 1.86 mmol.g-1. Water uptake, swelling, oxidative stability and methanol permeability of SPPEK- DMs membranes were investigated. SPPEK-DMs membranes exhibited high oxidative stability. The methanol permeability values of SPPEK-DMs membranes were in the range 5.15× 10^-8-6.61×10^-7 cm^2.s-1, which was much lower than those of Nafion117. The proton conductivity of SPPEK-DM40 membranes was 1.1 ×10^-2 S.cm^-1 at 70℃.展开更多
In order to effectively improve the properties of anion exchange membrane(AEM)materials,a series of novel poly(aryl ether nitrile)s with flexible side-chain-type quaternary phosphonium cations(PAEN-TPP-x)were designed...In order to effectively improve the properties of anion exchange membrane(AEM)materials,a series of novel poly(aryl ether nitrile)s with flexible side-chain-type quaternary phosphonium cations(PAEN-TPP-x)were designed and prepared on the basis of considering the influences of polymer backbone,cationic group species and the connection way between the cations and polymer chains.The synthetic method,structure and ion-exchange capacity,water absorption,swelling,hydroxide conductivity and alkaline stability of the obtained AEMs were studied.A comparative study with other reported AEMs was also performed for further exploration of the relationship between the structure and properties.These AEMs with flexible side-chain-type quaternary phosphonium cations displayed good comprehensive properties.Their water uptakes and swelling ratios were in the range of 11.6%–22.7%and 4.4%–7.8%at 60℃,respectively.They had hydroxide conductivity in the range of 28.6–45.8 mS cm^-1 at 60℃.Moreover,these AEMs also exhibited improved alkaline stability,and the hydroxide conductivity for PAEN-TPP-0.35 could remain 82.1%and 80.6%of its initial value at 60 and 90℃in 2 mol L^-1 NaOH solution for480 h,respectively.展开更多
A series ofpoly(aryl ether sulfone ketone)s containing phthalazinone and biphenyl moieties were synthesized by aromatic nucleophilic displacement polycondensation of 4-(4-hydroxylphenyl)(2H)-phthalazin-l-one (D...A series ofpoly(aryl ether sulfone ketone)s containing phthalazinone and biphenyl moieties were synthesized by aromatic nucleophilic displacement polycondensation of 4-(4-hydroxylphenyl)(2H)-phthalazin-l-one (DHPZ), 4,4'- dichlorobenzophenone (DCB), 4,4'-dichlorodiphenyl sulfone (DCS) and 4,4'-biphenol (BP) in different molar ratios. The obtained copolymers were characterized by different instrumental techniques (FTIR, TGA, DSC, WAXD, etc.). The inherent viscosities of these polymers were in the range of 0.43-0.56 dL g^-1. They were amorphous and had good solubility in polar aprotic organic solvents. The copolymers exhibited high glass transition temperatures (TgS) between 225℃ and 256℃and excellent thermal stability up to 517-526℃ (thermal decomposition temperatures for 5% weight loss, Td, 5%) in nitrogen. The tensile strength and elongation at break of the polymers ranged from 63 MPa to 71 MPa and from 18% to 21%, respectively. The processability of the material was effectively improved by the introduction of biphenyl group into polymer backbone.展开更多
Hydrophilic surface modification of poly(phthalazinone ether sulfone ketone)(PPESK) porous membranes was achieved via surface-initiated atom transfer radical polymerization(ATRP) in aqueous medium.Prior to ATRP.chloro...Hydrophilic surface modification of poly(phthalazinone ether sulfone ketone)(PPESK) porous membranes was achieved via surface-initiated atom transfer radical polymerization(ATRP) in aqueous medium.Prior to ATRP.chloromethyl groups were introduced onto PPESK main chains by chloromethylation.Chloromethvlated PPESK(CMPPESK) was fabricated into porous membrane through phase inversion technique.Hydrophilic poly(poly(ethylene glycol) methyl ether methacrylate)(P(PEGMA)) brushes were grafted from CMPPESK membrane ...展开更多
A new interfacial polymerization (IP) procedure is developed in order to synthesize polypiperazine-amide thin-film membrane on the inner surface of poly(phthalazinone ether sulfone ketone) (PPESK) hollow fiber u...A new interfacial polymerization (IP) procedure is developed in order to synthesize polypiperazine-amide thin-film membrane on the inner surface of poly(phthalazinone ether sulfone ketone) (PPESK) hollow fiber ultrafiltration (UF) membrane. A hollow fiber composite membrane with good performance was prepared and studied by PT-IR and scanning electron microscopy.展开更多
Preparation of an amphiphilic graft copolymer having poly(phthalazinone ether sulfone ketone)(PPESK) as main chains was carried out by atom transfer radical polymerization(ATRP).The precursor,chloromethylated PPESK (C...Preparation of an amphiphilic graft copolymer having poly(phthalazinone ether sulfone ketone)(PPESK) as main chains was carried out by atom transfer radical polymerization(ATRP).The precursor,chloromethylated PPESK (CMPPESK),was prepared by using chioromethylether as chloromethylation agent.Then,poly(ethylene glycol) methyl ether methacrylate(PEGMA) was used as monomer to synthesize PPESK-g-P(PEGMA) by ATRP method under the catalysis of a cuprous chloride/2,2'-bipyridyl system.PPESK/PPESK-g-P(PEGMA) blend m...展开更多
文摘Block copolymers with different backbone compositions have been prepared by the condensation of dimethylamino terminated poly(dimethylsiloxane) (PDMS) and hydroquinone terminated poly(phthalazinone ether nitrile) (PPEN) in the presence of chlorobenzcne/N-methyl pyrrolidone (NMP) as solvents. The products were characterized by FTIR, ^1H NMR and gel permeation chromatography. Differential scanning calorimetry analysis indicated that the block copolymers showed separated microphase.
文摘A series of novel poly(aryl ether nitrile)s containing phthalazinone moiety were synthesized by the nucleophilic displacement reaction of bisphenol-like monomers (I) with 2,6-difluorobenzonitrile. The inherent viscosities ranged from 0.46 to 1.07 dL g^-1. The glass transition temperatures were in the range of 277-295℃, and the temperatures for 10% weight loss in nitrogen atmosphere were found between 495 and 527 ℃. The structures of these resultant polymers were confirmed by FT-IR and 1^H NMR. Moreover, the properties of poly(aryl ether nitrile)s including solubility and crystallinity were also studied.
基金partly financed by the Major State Basic Research Development Program of China(No.2003 CB615700)the National Natural Science Foundation of China(No.20604005).
文摘Chloromethylated poly(phthalazinone ether sulfone ketone) (CMPPESK) was prepared from poly(phthalazinone ether sulfone ketone) (PPESK) using chloromethyl octyl ethers (CMOE) with lower toxicity as chloromethylated regent. CMPPESK was soluble in N-methyl-2-pyrrolidone (NMP), N,N-dimethylacetamide (DMAc) and chloroform. Quaternized poly(phthalazinone ether sulfone ketone) (QAPPESK) was prepared from CMPPESK by quaternization. QAPPESK had excellent solvent resistance, which was only partly soluble in sulfuric acid (98%) and swollen in N,N-dimethylformamide (DMF). The vanadium redox flow battery (V-RFB) using QAPPESK anion-exchange membrane had better performance with 88.3% of overall energy efficiency.
文摘Two novel heterocyclic diamine monomers: 1,2-dihydro-2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl] (2H)phthalazin-1-one and 1,2-dihydro-2-(4-aminophenyl)-4-[4-(4-aminophenoxy)-3,5-dimethylphenyl](2H)phthalazin-1-one were successfully synthesized from readily available heterocyclic bisphenol-like monomers in two steps in high yield. A series of novel poly(aryl ether amide)s containing the phthalazinone moiety were successfully prepared by the direct polymerization of the novel diamines and aromatic dicarboxylic acids using triphenyl phosphite and pyridine as condensing agents.
文摘A novel series of poly(aryl ether sulfone ketone)s (PPESKs) containing phthalazinone and biphenyl moieties were prepared by two-step nucleophilic polycondensation reaction. The ^-Mw values of these copolymers were between 38,330 and 67,900. The glass transition temperatures (Tg) and 5% decomposition temperatures were ranged in 253-269 ℃ and 488-500 ℃, respectively, The structures of these copolymers were confirmed by FT-IR and ^1H NMR. Moreover, all the resultant copolymers were amorphous determined by wide angle X-ray diffraction (WAXD).
基金the National Natural Science Foundation of China for financial support.
文摘1, 2-Diliydro-4-(4-hydroxyphenyl)(2H)phthalazin-1-one(DHPZ) was sulfonated in concentrated Sulfuric acid. Poly(phthalazinone ether ketone) containing pendant sodium sulfonate group was synthesized from sulfonated and pure 1,2-dihydro-4-(4-hydroxyphenyl)(2H)phthalazin-1-one, and 4,4'-difluorodiphenylketone. The sulfonated monomer and sulfonated polymer were characterized with FT-IR and H-1-NMR.
基金This work was sponsored by the National Natural Science Foundation of China (No. 59473901).
文摘Three novel poly(ether imide)s were synthesized by one-step solution polymerization from 2-(3, 4-dicarboxyl-N-phenyl)-4-(3, 4-dicarboxyl-phenoxyl-4-(2-methyl)-phenyl)-2, 3- phthal-azin-1-one dianhydride and three amines, and characterized. The polymers show good solubility and thermal properties.
基金This project was financially supported by National High Technology and Development Program of China(863 Program)(No.2003AA33G030)
文摘Trimethoxysilyl-functionalized PPEK(PKGS) films had been designed to serve as wear resistant coatings for silicon surfaces. These surface films were formed by a dip-coating technique applied to self-assembled monolayers(SAMs).The formation and wetting behavior of PKGS films were characterized by means of contact angle measurement.The friction coefficient of the film prepared is very low(about 0.1),and the anti-wear behavior is good,with a lack of failure after sliding over 1800 s.
文摘A novel poly(ether imide)s containing phthalazinone and isopropyl moieties derived from 2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl]-phthalazin-1-one and bisphenol-A diphthalic anhydride was synthesized by one-step solution condensation polymerization in nr-cresol. The polymer was characterized by FTIR, NMR, molecular weights, glass transition temperature, thermal degradation temperature and WAXD.
文摘A novel alkoxysilyl-functionalized poly(phthalazinone ether ketone) (PPEK) was prepared for the boundary lubricant application in micro-electro-mechanical system (MEMS). The synthesis of functionalized PPEK was started from the hydroxylation of PPEK, then following with the corresponding ring-opening reaction of 3-glycidoxypropyltrimethoxysilane (GPTMS). The structures of the functional PPEK were confirmed by FTIR, 1H NMR, 29Si NMR, and UV–vis spectrum.
基金supported by the National Natural Science Foundation of China(Nos.50673031 and 50973036)
文摘Based on several unsymmetrical, twist, noncoplanar phthalazinone-containing monomers 2a-2e and an active bis(4-fluorophenyl)phenyl phosphine oxide (BFPPO) monomer, a series of novel poly(phthalazinone ether phosphine oxide)s (PPEPO) was synthesized by anhydrous K2CO3 mediated N-C coupling reaction in DMAc. The polymers exhibited good thermal properties with Tgs ranging from 267℃ to 306℃ and 5% weight loss temperatures in nitrogen higher than 430℃, together with high char yield upon prolonged heating at 800℃ (35%-56%). Moreover, the polymers were readily soluble in common organic solvents, such as N-methyl-2-pyrrolidone, chloroform and m-cresol. These polymers had inherent viscosities in the range of 0.45-0.72 dL/g and could be cast into flexible and colorless films by spin coating or casting approach.
基金This project is financially supported by Hi-tech Research and Development Program(2003AA33g-030)the National Natural Science Foundation of China(Contract grant number:50143013).
文摘A novel aromatic diamine, 1, 2-dihydro-2-(4-aminophenyl)-4-[3-methoxy-4-(4-aminophenoxy)]-2, 3-phthalazin-l-one (OO-DA) containing aza heterocyclic structure was synthesized from the bisphenol-like monomer in two steps and used for preparing new aromatic polyamides with high inherent viscosity of 0.89-1.03 dL.g^-1. The structures of diamine and polymers obtained were confirmed by MS, PT-IR, WAXD and ^1H-NMR. The synthesized polymers exhibited high glass transition temperature in the range of 281-307℃ and good solubility in polar solvents.
基金the National Natural Science Foundation of China(No.21978237)Natural Science Foundation of Shaanxi Province(Nos.2023-JC-YB-370 and 2024-JC-YBQN-0140)Shaanxi Fundamental Science Research Project for Chemistry and Biology(No.22JHQ032)are gratefully acknowledged.
文摘Dielectric energy storage materials that are extensively employed in capacitors and other electronic devices have attracted increasing attentions amid the rapid progress of electronic technology.However,the commercialized polymeric and ceramic dielectric materials characterized by low energy storage density face numerous limitations in practical applications.In this study,we report the simultaneous enhancement of dielectric properties of poly(arylene ether nitrile)(PEN)through the incorporating of sulfonated PEN(SPEN)modified barium titanate nanorods(BTNR)(SPEN@BTNR)and hot-stretching.BTNR is synthesized using a two-step hydrothermal method,aminated with KH550,and then reacted with SPEN to form the cladding-modified SPEN@BTNR.Due to the intrinsic high permittivity of barium titanate(BT)and enhanced compatibility between SPEN@BTNR and PEN stemming from the cladding of SPEN,the dielectric constant and breakdown strength of SPEN@BTNR/PEN composite are as high as 14.0 at 103 Hz and 198.1 kV/mm at the doping amount of 15 wt.%,respectively.As a result,the energy storage density of SPEN@BTNR/PEN is increased to 2.43 J/cm^(3),compared with that of 0.82 J/cm^(3)for PEN.In addition,derived from the rearrangement of SPEN@BTNR and orientation of PEN after hot-stretching,the dielectric constant and breakdown strength of SPEN@BTNR/PEN with 15 wt.%fillers are further enhanced to 17.1 and 204.8 kV/mm,respectively,resulting in an energy storage density of 3.36 J/cm^(3).The boosting of energy storage density up to 310%provides a new idea for improving the performances of dielectric energy storage materials.
基金supported by the Natural Science Foundation of Liaoning Province of China(No.20041076)
文摘Sulfonated poly(ether ketone)s containing 3,5-dimethyl phthalazinone moieties (SPPEK-DMs) with different degrees of sulfonation (DS) were synthesized via direct polycondensation from 4-(3,5-dimethyl-4-hydroxyphenyl)-2,3- phthalazinone, 4,4'-difluorobenzophenone and 3,3'-disulfonate-4,4'-difluorobenzophenone. The chemical structure of SPPEK-DMs was characterized by FTIR and 1H-NMR. Thermal stability of SPPEK-DMs was characterized by the thermogravimetric analysis. The membranes prepared from SPPEK-DMs exhibited ion exchange capacities (IEC) ranging from 0.93 mmol.g-1 to 1.86 mmol.g-1. Water uptake, swelling, oxidative stability and methanol permeability of SPPEK- DMs membranes were investigated. SPPEK-DMs membranes exhibited high oxidative stability. The methanol permeability values of SPPEK-DMs membranes were in the range 5.15× 10^-8-6.61×10^-7 cm^2.s-1, which was much lower than those of Nafion117. The proton conductivity of SPPEK-DM40 membranes was 1.1 ×10^-2 S.cm^-1 at 70℃.
基金supported by the National Natural Science Foundation of China (21404016)the Key Research Program of Jiangsu Province (BE2017645)+1 种基金the Six Talent Peaks Project of Jiangsu Province (XCL-078)a project funded by the Priority Academic Program Development of Jiangsu Higher Education Institutions of China
文摘In order to effectively improve the properties of anion exchange membrane(AEM)materials,a series of novel poly(aryl ether nitrile)s with flexible side-chain-type quaternary phosphonium cations(PAEN-TPP-x)were designed and prepared on the basis of considering the influences of polymer backbone,cationic group species and the connection way between the cations and polymer chains.The synthetic method,structure and ion-exchange capacity,water absorption,swelling,hydroxide conductivity and alkaline stability of the obtained AEMs were studied.A comparative study with other reported AEMs was also performed for further exploration of the relationship between the structure and properties.These AEMs with flexible side-chain-type quaternary phosphonium cations displayed good comprehensive properties.Their water uptakes and swelling ratios were in the range of 11.6%–22.7%and 4.4%–7.8%at 60℃,respectively.They had hydroxide conductivity in the range of 28.6–45.8 mS cm^-1 at 60℃.Moreover,these AEMs also exhibited improved alkaline stability,and the hydroxide conductivity for PAEN-TPP-0.35 could remain 82.1%and 80.6%of its initial value at 60 and 90℃in 2 mol L^-1 NaOH solution for480 h,respectively.
基金financially supported by the National Natural Science Foundation of the China(No.50703004)
文摘A series ofpoly(aryl ether sulfone ketone)s containing phthalazinone and biphenyl moieties were synthesized by aromatic nucleophilic displacement polycondensation of 4-(4-hydroxylphenyl)(2H)-phthalazin-l-one (DHPZ), 4,4'- dichlorobenzophenone (DCB), 4,4'-dichlorodiphenyl sulfone (DCS) and 4,4'-biphenol (BP) in different molar ratios. The obtained copolymers were characterized by different instrumental techniques (FTIR, TGA, DSC, WAXD, etc.). The inherent viscosities of these polymers were in the range of 0.43-0.56 dL g^-1. They were amorphous and had good solubility in polar aprotic organic solvents. The copolymers exhibited high glass transition temperatures (TgS) between 225℃ and 256℃and excellent thermal stability up to 517-526℃ (thermal decomposition temperatures for 5% weight loss, Td, 5%) in nitrogen. The tensile strength and elongation at break of the polymers ranged from 63 MPa to 71 MPa and from 18% to 21%, respectively. The processability of the material was effectively improved by the introduction of biphenyl group into polymer backbone.
基金supported by the National Basic Research Program of China(No2009CB623402)China Postdoctoral Science Foundation(No20080430220)
文摘Hydrophilic surface modification of poly(phthalazinone ether sulfone ketone)(PPESK) porous membranes was achieved via surface-initiated atom transfer radical polymerization(ATRP) in aqueous medium.Prior to ATRP.chloromethyl groups were introduced onto PPESK main chains by chloromethylation.Chloromethvlated PPESK(CMPPESK) was fabricated into porous membrane through phase inversion technique.Hydrophilic poly(poly(ethylene glycol) methyl ether methacrylate)(P(PEGMA)) brushes were grafted from CMPPESK membrane ...
文摘A new interfacial polymerization (IP) procedure is developed in order to synthesize polypiperazine-amide thin-film membrane on the inner surface of poly(phthalazinone ether sulfone ketone) (PPESK) hollow fiber ultrafiltration (UF) membrane. A hollow fiber composite membrane with good performance was prepared and studied by PT-IR and scanning electron microscopy.
基金supported by the"973"program of China(No.2009CB623402)Engineering Research Center of Ministry of Education of China(No.JD09011)
文摘Preparation of an amphiphilic graft copolymer having poly(phthalazinone ether sulfone ketone)(PPESK) as main chains was carried out by atom transfer radical polymerization(ATRP).The precursor,chloromethylated PPESK (CMPPESK),was prepared by using chioromethylether as chloromethylation agent.Then,poly(ethylene glycol) methyl ether methacrylate(PEGMA) was used as monomer to synthesize PPESK-g-P(PEGMA) by ATRP method under the catalysis of a cuprous chloride/2,2'-bipyridyl system.PPESK/PPESK-g-P(PEGMA) blend m...